Electroless Ni–B Coating Formed from a Stabilizer-Free Double Bath
Abstract The present work investigates the deposition of nickel boron coatings by electroless method. A double bath scheme was adopted, and the bath temperature was also varied to get coatings in different boron range. The double bath coatings have higher microhardness, scratch hardness, wear and corrosion resistance compared to single bath deposits. The double bath scheme led to the formation of coatings with a compact crack-free morphology except at 95 °C bath temperature. The improvement in hardness was 16.85, 11.43 and 10% at 85, 90 and 95 °C bath temperature compared to the single bath coatings. The increase in scratch hardness was within 20–22%. A higher corrosion potential of − 180 and − 178 mV was also seen..
Medienart: |
E-Artikel |
---|
Erscheinungsjahr: |
2024 |
---|---|
Erschienen: |
2024 |
Enthalten in: |
Zur Gesamtaufnahme - volume:77 |
---|---|
Enthalten in: |
Transactions of the Indian Institute of Metals - 77(2024), 4 vom: 04. Jan., Seite 1039-1051 |
Sprache: |
Englisch |
---|
Beteiligte Personen: |
Agrawal, Rohit [VerfasserIn] |
---|
Links: |
Volltext [lizenzpflichtig] |
---|
Themen: |
Corrosion analysis |
---|
Anmerkungen: |
© The Indian Institute of Metals - IIM 2024. Springer Nature or its licensor (e.g. a society or other partner) holds exclusive rights to this article under a publishing agreement with the author(s) or other rightsholder(s); author self-archiving of the accepted manuscript version of this article is solely governed by the terms of such publishing agreement and applicable law. |
---|
doi: |
10.1007/s12666-023-03220-9 |
---|
funding: |
|
---|---|
Förderinstitution / Projekttitel: |
|
PPN (Katalog-ID): |
SPR055271308 |
---|
LEADER | 01000naa a22002652 4500 | ||
---|---|---|---|
001 | SPR055271308 | ||
003 | DE-627 | ||
005 | 20240325061007.0 | ||
007 | cr uuu---uuuuu | ||
008 | 240325s2024 xx |||||o 00| ||eng c | ||
024 | 7 | |a 10.1007/s12666-023-03220-9 |2 doi | |
035 | |a (DE-627)SPR055271308 | ||
035 | |a (SPR)s12666-023-03220-9-e | ||
040 | |a DE-627 |b ger |c DE-627 |e rakwb | ||
041 | |a eng | ||
082 | 0 | 4 | |a 620 |a 660 |a 670 |q VZ |
100 | 1 | |a Agrawal, Rohit |e verfasserin |4 aut | |
245 | 1 | 0 | |a Electroless Ni–B Coating Formed from a Stabilizer-Free Double Bath |
264 | 1 | |c 2024 | |
336 | |a Text |b txt |2 rdacontent | ||
337 | |a Computermedien |b c |2 rdamedia | ||
338 | |a Online-Ressource |b cr |2 rdacarrier | ||
500 | |a © The Indian Institute of Metals - IIM 2024. Springer Nature or its licensor (e.g. a society or other partner) holds exclusive rights to this article under a publishing agreement with the author(s) or other rightsholder(s); author self-archiving of the accepted manuscript version of this article is solely governed by the terms of such publishing agreement and applicable law. | ||
520 | |a Abstract The present work investigates the deposition of nickel boron coatings by electroless method. A double bath scheme was adopted, and the bath temperature was also varied to get coatings in different boron range. The double bath coatings have higher microhardness, scratch hardness, wear and corrosion resistance compared to single bath deposits. The double bath scheme led to the formation of coatings with a compact crack-free morphology except at 95 °C bath temperature. The improvement in hardness was 16.85, 11.43 and 10% at 85, 90 and 95 °C bath temperature compared to the single bath coatings. The increase in scratch hardness was within 20–22%. A higher corrosion potential of − 180 and − 178 mV was also seen. | ||
650 | 4 | |a Electroless Ni–B |7 (dpeaa)DE-He213 | |
650 | 4 | |a Replenishment |7 (dpeaa)DE-He213 | |
650 | 4 | |a Tribological behaviour |7 (dpeaa)DE-He213 | |
650 | 4 | |a Microhardness |7 (dpeaa)DE-He213 | |
650 | 4 | |a Corrosion analysis |7 (dpeaa)DE-He213 | |
700 | 1 | |a Gupta, Lokesh |4 aut | |
700 | 1 | |a Jain, Siddharth |4 aut | |
700 | 1 | |a Sharma, Ritik |4 aut | |
700 | 1 | |a Mukhopadhyay, Arkadeb |0 (orcid)0000-0002-4942-722X |4 aut | |
773 | 0 | 8 | |i Enthalten in |t Transactions of the Indian Institute of Metals |d Springer India, 2008 |g 77(2024), 4 vom: 04. Jan., Seite 1039-1051 |w (DE-627)SPR026759160 |w (DE-600)2535335-4 |x 0975-1645 |7 nnns |
773 | 1 | 8 | |g volume:77 |g year:2024 |g number:4 |g day:04 |g month:01 |g pages:1039-1051 |
856 | 4 | 0 | |u https://dx.doi.org/10.1007/s12666-023-03220-9 |z lizenzpflichtig |3 Volltext |
912 | |a GBV_SPRINGER | ||
912 | |a SSG-OLC-PHA | ||
951 | |a AR | ||
952 | |d 77 |j 2024 |e 4 |b 04 |c 01 |h 1039-1051 |