Effectiveness of sodium hypochlorite and sulfinic acid sodium salt treatment on dentin-resin bonding : Long-term durability of one-step self-etching adhesive
This study aimed to evaluate the effect of sulfinic acid sodium salt interposition after acid and sodium hypochlorite treatment (NC treatment) on dentin bonding durability using a mild type one-step self-etching adhesive. Fifteen human third molars were randomly assigned into three experimental groups according to dentin pretreatment before applying the one-step self-etching adhesive: Cont group, without pretreatment; NC group, pretreatment with phosphoric acid and sodium hypochlorite gel; and NC+AC group, additional treatment with sulfinic acid sodium salt followed by the same pretreatment of the NC group. Microtensile bond strength was measured and the pre-treated dentin surface, fracture modes, and bonding interface were observed. The bond strength of the NC+AC group was significantly higher than that of the other groups (p<0.001). The dentin-adhesive interface was degraded after 1 year only in the Cont group. Our results demonstrated NC treatment improves bonding durability and application of sodium sulfinic acid salt after NC treatment improves bonding effectiveness.
Medienart: |
E-Artikel |
---|
Erscheinungsjahr: |
2017 |
---|---|
Erschienen: |
2017 |
Enthalten in: |
Zur Gesamtaufnahme - volume:36 |
---|---|
Enthalten in: |
Dental materials journal - 36(2017), 6 vom: 29. Nov., Seite 842-850 |
Sprache: |
Englisch |
---|
Beteiligte Personen: |
Nakatani, Hayaki [VerfasserIn] |
---|
Links: |
---|
Anmerkungen: |
Date Completed 24.09.2018 Date Revised 24.09.2018 published: Print-Electronic Citation Status MEDLINE |
---|
doi: |
10.4012/dmj.2017-105 |
---|
funding: |
|
---|---|
Förderinstitution / Projekttitel: |
|
PPN (Katalog-ID): |
NLM277492203 |
---|
LEADER | 01000naa a22002652 4500 | ||
---|---|---|---|
001 | NLM277492203 | ||
003 | DE-627 | ||
005 | 20231225014330.0 | ||
007 | cr uuu---uuuuu | ||
008 | 231225s2017 xx |||||o 00| ||eng c | ||
024 | 7 | |a 10.4012/dmj.2017-105 |2 doi | |
028 | 5 | 2 | |a pubmed24n0924.xml |
035 | |a (DE-627)NLM277492203 | ||
035 | |a (NLM)29081450 | ||
040 | |a DE-627 |b ger |c DE-627 |e rakwb | ||
041 | |a eng | ||
100 | 1 | |a Nakatani, Hayaki |e verfasserin |4 aut | |
245 | 1 | 0 | |a Effectiveness of sodium hypochlorite and sulfinic acid sodium salt treatment on dentin-resin bonding |b Long-term durability of one-step self-etching adhesive |
264 | 1 | |c 2017 | |
336 | |a Text |b txt |2 rdacontent | ||
337 | |a ƒaComputermedien |b c |2 rdamedia | ||
338 | |a ƒa Online-Ressource |b cr |2 rdacarrier | ||
500 | |a Date Completed 24.09.2018 | ||
500 | |a Date Revised 24.09.2018 | ||
500 | |a published: Print-Electronic | ||
500 | |a Citation Status MEDLINE | ||
520 | |a This study aimed to evaluate the effect of sulfinic acid sodium salt interposition after acid and sodium hypochlorite treatment (NC treatment) on dentin bonding durability using a mild type one-step self-etching adhesive. Fifteen human third molars were randomly assigned into three experimental groups according to dentin pretreatment before applying the one-step self-etching adhesive: Cont group, without pretreatment; NC group, pretreatment with phosphoric acid and sodium hypochlorite gel; and NC+AC group, additional treatment with sulfinic acid sodium salt followed by the same pretreatment of the NC group. Microtensile bond strength was measured and the pre-treated dentin surface, fracture modes, and bonding interface were observed. The bond strength of the NC+AC group was significantly higher than that of the other groups (p<0.001). The dentin-adhesive interface was degraded after 1 year only in the Cont group. Our results demonstrated NC treatment improves bonding durability and application of sodium sulfinic acid salt after NC treatment improves bonding effectiveness | ||
650 | 4 | |a Journal Article | |
650 | 4 | |a Dentin bonding durability | |
650 | 4 | |a Microtensile bond strength | |
650 | 4 | |a Mild type one-step self-etching adhesive | |
650 | 4 | |a Sodium hypochlorite | |
650 | 4 | |a Sulfinic acid sodium salt | |
650 | 7 | |a Dental Materials |2 NLM | |
650 | 7 | |a Dentin-Bonding Agents |2 NLM | |
650 | 7 | |a Resins, Synthetic |2 NLM | |
650 | 7 | |a Sulfinic Acids |2 NLM | |
650 | 7 | |a Sodium Hypochlorite |2 NLM | |
650 | 7 | |a DY38VHM5OD |2 NLM | |
700 | 1 | |a Mine, Atsushi |e verfasserin |4 aut | |
700 | 1 | |a Matsumoto, Mariko |e verfasserin |4 aut | |
700 | 1 | |a Kabetani, Tomoshige |e verfasserin |4 aut | |
700 | 1 | |a Kawaguchi-Uemura, Asuka |e verfasserin |4 aut | |
700 | 1 | |a Higashi, Mami |e verfasserin |4 aut | |
700 | 1 | |a Tajiri, Yuko |e verfasserin |4 aut | |
700 | 1 | |a Imai, Dai |e verfasserin |4 aut | |
700 | 1 | |a Hagino, Ryosuke |e verfasserin |4 aut | |
700 | 1 | |a Minamino, Takuya |e verfasserin |4 aut | |
700 | 1 | |a Miura, Jiro |e verfasserin |4 aut | |
700 | 1 | |a Yatani, Hirofumi |e verfasserin |4 aut | |
773 | 0 | 8 | |i Enthalten in |t Dental materials journal |d 1985 |g 36(2017), 6 vom: 29. Nov., Seite 842-850 |w (DE-627)NLM012859230 |x 1881-1361 |7 nnns |
773 | 1 | 8 | |g volume:36 |g year:2017 |g number:6 |g day:29 |g month:11 |g pages:842-850 |
856 | 4 | 0 | |u http://dx.doi.org/10.4012/dmj.2017-105 |3 Volltext |
912 | |a GBV_USEFLAG_A | ||
912 | |a GBV_NLM | ||
951 | |a AR | ||
952 | |d 36 |j 2017 |e 6 |b 29 |c 11 |h 842-850 |