Ytterbium-doped large-mode-area silica fiber fabricated by using chelate precursor doping technique
We reported on a highly effective chelate precursor doping technique for Yb-doped large-mode-area (LMA) fiber manufacture. By accurately controlling the evaporation temperature and flow rate of carrier gas, the chelate precursor doping technique is capable of making Yb-doped LMA silica fiber with good uniformity free of center dip, low numerical aperture of ~0.056, large preform core size of 4.46 mm, and appropriate cladding absorption of 1.17 dB/m at 976.4 nm. Based on a single-end-pump all-fiber oscillator laser setup, the laser output at 1080 nm reached 700 W with slope efficiency of 54.2%.
Medienart: |
E-Artikel |
---|
Erscheinungsjahr: |
2014 |
---|---|
Erschienen: |
2014 |
Enthalten in: |
Zur Gesamtaufnahme - volume:53 |
---|---|
Enthalten in: |
Applied optics - 53(2014), 15 vom: 20. Mai, Seite 3191-5 |
Sprache: |
Englisch |
---|
Beteiligte Personen: |
Shi, Tengfei [VerfasserIn] |
---|
Links: |
---|
Themen: |
---|
Anmerkungen: |
Date Completed 21.05.2015 Date Revised 23.10.2018 published: Print Citation Status PubMed-not-MEDLINE |
---|
doi: |
10.1364/AO.53.003191 |
---|
funding: |
|
---|---|
Förderinstitution / Projekttitel: |
|
PPN (Katalog-ID): |
NLM239117565 |
---|
LEADER | 01000naa a22002652 4500 | ||
---|---|---|---|
001 | NLM239117565 | ||
003 | DE-627 | ||
005 | 20231224115243.0 | ||
007 | cr uuu---uuuuu | ||
008 | 231224s2014 xx |||||o 00| ||eng c | ||
024 | 7 | |a 10.1364/AO.53.003191 |2 doi | |
028 | 5 | 2 | |a pubmed24n0797.xml |
035 | |a (DE-627)NLM239117565 | ||
035 | |a (NLM)24922203 | ||
040 | |a DE-627 |b ger |c DE-627 |e rakwb | ||
041 | |a eng | ||
100 | 1 | |a Shi, Tengfei |e verfasserin |4 aut | |
245 | 1 | 0 | |a Ytterbium-doped large-mode-area silica fiber fabricated by using chelate precursor doping technique |
264 | 1 | |c 2014 | |
336 | |a Text |b txt |2 rdacontent | ||
337 | |a ƒaComputermedien |b c |2 rdamedia | ||
338 | |a ƒa Online-Ressource |b cr |2 rdacarrier | ||
500 | |a Date Completed 21.05.2015 | ||
500 | |a Date Revised 23.10.2018 | ||
500 | |a published: Print | ||
500 | |a Citation Status PubMed-not-MEDLINE | ||
520 | |a We reported on a highly effective chelate precursor doping technique for Yb-doped large-mode-area (LMA) fiber manufacture. By accurately controlling the evaporation temperature and flow rate of carrier gas, the chelate precursor doping technique is capable of making Yb-doped LMA silica fiber with good uniformity free of center dip, low numerical aperture of ~0.056, large preform core size of 4.46 mm, and appropriate cladding absorption of 1.17 dB/m at 976.4 nm. Based on a single-end-pump all-fiber oscillator laser setup, the laser output at 1080 nm reached 700 W with slope efficiency of 54.2% | ||
650 | 4 | |a Journal Article | |
700 | 1 | |a Zhou, Zhiguang |e verfasserin |4 aut | |
700 | 1 | |a Ni, Li |e verfasserin |4 aut | |
700 | 1 | |a Xiao, Xusheng |e verfasserin |4 aut | |
700 | 1 | |a Zhan, Huan |e verfasserin |4 aut | |
700 | 1 | |a Zhang, Aidong |e verfasserin |4 aut | |
700 | 1 | |a Lin, Aoxiang |e verfasserin |4 aut | |
773 | 0 | 8 | |i Enthalten in |t Applied optics |d 1966 |g 53(2014), 15 vom: 20. Mai, Seite 3191-5 |w (DE-627)NLM114401330 |x 1539-4522 |7 nnns |
773 | 1 | 8 | |g volume:53 |g year:2014 |g number:15 |g day:20 |g month:05 |g pages:3191-5 |
856 | 4 | 0 | |u http://dx.doi.org/10.1364/AO.53.003191 |3 Volltext |
912 | |a GBV_USEFLAG_A | ||
912 | |a GBV_NLM | ||
951 | |a AR | ||
952 | |d 53 |j 2014 |e 15 |b 20 |c 05 |h 3191-5 |