A stable PEO-tethered PDMS surface having controllable wetting property by a swelling-deswelling process
A PEO-tethered layer on a PDMS (polydimethylsiloxane) cross-linked network has been prepared by a swelling-deswelling process. During swelling, the PDMS block of a PDMS-b-PEO diblock copolymer penetrates into the PDMS substrate and interacts with PDMS chains because of the van der Waals force and hydrophobic interaction between them. Upon deswelling, the PDMS block is trapped in the PDMS matrix while the PEO, as a hydrophilic block, is tethered to the surface. The PEO-tethered layer showed stability when treated in water for 16 h. The surface fraction of PEO and the wetting property of the PEO-tethered PDMS surface can be controlled by the cross linking density of the PDMS matrix. A patterned PEO-tethered layer on a PDMS network was also created by microcontact printing and water condensation figures (CFs) were used to study the patterned surface with different wetting properties.
Medienart: |
E-Artikel |
---|
Erscheinungsjahr: |
2006 |
---|---|
Erschienen: |
2006 |
Enthalten in: |
Zur Gesamtaufnahme - volume:2 |
---|---|
Enthalten in: |
Soft matter - 2(2006), 8 vom: 20. Juli, Seite 705-709 |
Sprache: |
Englisch |
---|
Beteiligte Personen: |
Yu, Kai [VerfasserIn] |
---|
Links: |
---|
Themen: |
---|
Anmerkungen: |
Date Revised 20.07.2020 published: Print Citation Status PubMed-not-MEDLINE |
---|
doi: |
10.1039/b602880m |
---|
funding: |
|
---|---|
Förderinstitution / Projekttitel: |
|
PPN (Katalog-ID): |
NLM31256564X |
---|
LEADER | 01000naa a22002652 4500 | ||
---|---|---|---|
001 | NLM31256564X | ||
003 | DE-627 | ||
005 | 20231225144702.0 | ||
007 | cr uuu---uuuuu | ||
008 | 231225s2006 xx |||||o 00| ||eng c | ||
024 | 7 | |a 10.1039/b602880m |2 doi | |
028 | 5 | 2 | |a pubmed24n1041.xml |
035 | |a (DE-627)NLM31256564X | ||
035 | |a (NLM)32680229 | ||
040 | |a DE-627 |b ger |c DE-627 |e rakwb | ||
041 | |a eng | ||
100 | 1 | |a Yu, Kai |e verfasserin |4 aut | |
245 | 1 | 2 | |a A stable PEO-tethered PDMS surface having controllable wetting property by a swelling-deswelling process |
264 | 1 | |c 2006 | |
336 | |a Text |b txt |2 rdacontent | ||
337 | |a ƒaComputermedien |b c |2 rdamedia | ||
338 | |a ƒa Online-Ressource |b cr |2 rdacarrier | ||
500 | |a Date Revised 20.07.2020 | ||
500 | |a published: Print | ||
500 | |a Citation Status PubMed-not-MEDLINE | ||
520 | |a A PEO-tethered layer on a PDMS (polydimethylsiloxane) cross-linked network has been prepared by a swelling-deswelling process. During swelling, the PDMS block of a PDMS-b-PEO diblock copolymer penetrates into the PDMS substrate and interacts with PDMS chains because of the van der Waals force and hydrophobic interaction between them. Upon deswelling, the PDMS block is trapped in the PDMS matrix while the PEO, as a hydrophilic block, is tethered to the surface. The PEO-tethered layer showed stability when treated in water for 16 h. The surface fraction of PEO and the wetting property of the PEO-tethered PDMS surface can be controlled by the cross linking density of the PDMS matrix. A patterned PEO-tethered layer on a PDMS network was also created by microcontact printing and water condensation figures (CFs) were used to study the patterned surface with different wetting properties | ||
650 | 4 | |a Journal Article | |
700 | 1 | |a Han, Yanchun |e verfasserin |4 aut | |
773 | 0 | 8 | |i Enthalten in |t Soft matter |d 2005 |g 2(2006), 8 vom: 20. Juli, Seite 705-709 |w (DE-627)NLM185552897 |x 1744-6848 |7 nnns |
773 | 1 | 8 | |g volume:2 |g year:2006 |g number:8 |g day:20 |g month:07 |g pages:705-709 |
856 | 4 | 0 | |u http://dx.doi.org/10.1039/b602880m |3 Volltext |
912 | |a GBV_USEFLAG_A | ||
912 | |a GBV_NLM | ||
951 | |a AR | ||
952 | |d 2 |j 2006 |e 8 |b 20 |c 07 |h 705-709 |