Preventive resin restorations vs. amalgam restorations : a three-year clinical study
A three-year clinical study was completed at the College of Dentistry comparing the overall performance of Class I amalgam restorations with preventive resin restorations (PRRs). Seventy-four PRRs and fifty-two amalgam restorations were placed in the posterior teeth of thirty-eight patients. The PRR was composed of two materials: P-50 (3M Corp.), a heavily filled composite resin, and White Sealant (3M Corp.), a light-cured sealant. Fast-set Dispersalloy (Johnson and Johnson Corp.) was used for the amalgam restorations. The restorations were evaluated at six months, one year, two years and three years. The USPHS/Ryge system was used to evaluate anatomic form, marginal adaptation, marginal discoloration and recurrent caries of both type restorations. A restoration was considered a failure if any part of the restoration was replaced due to secondary caries. There were two failures of PRRs at six months, and four failures at one year. Failures were due to non retention of the sealant of the PRR and possibly related to operator error. The failures were easily repaired and removed from the study. No PRR failed at the two or three year evaluations. No amalgam restoration failed within the three year period.
Medienart: |
Artikel |
---|
Erscheinungsjahr: |
1997 |
---|---|
Erschienen: |
1997 |
Enthalten in: |
Zur Gesamtaufnahme - volume:77 |
---|---|
Enthalten in: |
The Journal of the Tennessee Dental Association - 77(1997), 4 vom: 02. Okt., Seite 36-40 |
Sprache: |
Englisch |
---|
Beteiligte Personen: |
Cloyd, S [VerfasserIn] |
---|
Anmerkungen: |
Date Completed 16.06.1998 Date Revised 21.11.2013 published: Print Citation Status MEDLINE |
---|
Förderinstitution / Projekttitel: |
|
---|
PPN (Katalog-ID): |
NLM094622973 |
---|
LEADER | 01000naa a22002652 4500 | ||
---|---|---|---|
001 | NLM094622973 | ||
003 | DE-627 | ||
005 | 20231222100050.0 | ||
007 | tu | ||
008 | 231222s1997 xx ||||| 00| ||eng c | ||
028 | 5 | 2 | |a pubmed24n0316.xml |
035 | |a (DE-627)NLM094622973 | ||
035 | |a (NLM)9520761 | ||
040 | |a DE-627 |b ger |c DE-627 |e rakwb | ||
041 | |a eng | ||
100 | 1 | |a Cloyd, S |e verfasserin |4 aut | |
245 | 1 | 0 | |a Preventive resin restorations vs. amalgam restorations |b a three-year clinical study |
264 | 1 | |c 1997 | |
336 | |a Text |b txt |2 rdacontent | ||
337 | |a ohne Hilfsmittel zu benutzen |b n |2 rdamedia | ||
338 | |a Band |b nc |2 rdacarrier | ||
500 | |a Date Completed 16.06.1998 | ||
500 | |a Date Revised 21.11.2013 | ||
500 | |a published: Print | ||
500 | |a Citation Status MEDLINE | ||
520 | |a A three-year clinical study was completed at the College of Dentistry comparing the overall performance of Class I amalgam restorations with preventive resin restorations (PRRs). Seventy-four PRRs and fifty-two amalgam restorations were placed in the posterior teeth of thirty-eight patients. The PRR was composed of two materials: P-50 (3M Corp.), a heavily filled composite resin, and White Sealant (3M Corp.), a light-cured sealant. Fast-set Dispersalloy (Johnson and Johnson Corp.) was used for the amalgam restorations. The restorations were evaluated at six months, one year, two years and three years. The USPHS/Ryge system was used to evaluate anatomic form, marginal adaptation, marginal discoloration and recurrent caries of both type restorations. A restoration was considered a failure if any part of the restoration was replaced due to secondary caries. There were two failures of PRRs at six months, and four failures at one year. Failures were due to non retention of the sealant of the PRR and possibly related to operator error. The failures were easily repaired and removed from the study. No PRR failed at the two or three year evaluations. No amalgam restoration failed within the three year period | ||
650 | 4 | |a Clinical Trial | |
650 | 4 | |a Comparative Study | |
650 | 4 | |a Journal Article | |
650 | 7 | |a Composite Resins |2 NLM | |
650 | 7 | |a Dental Alloys |2 NLM | |
650 | 7 | |a Pit and Fissure Sealants |2 NLM | |
650 | 7 | |a P50 composite resin |2 NLM | |
650 | 7 | |a 117681-35-3 |2 NLM | |
650 | 7 | |a Dispersalloy |2 NLM | |
650 | 7 | |a 39323-76-7 |2 NLM | |
650 | 7 | |a Bisphenol A-Glycidyl Methacrylate |2 NLM | |
650 | 7 | |a 454I75YXY0 |2 NLM | |
650 | 7 | |a Dental Amalgam |2 NLM | |
650 | 7 | |a 8049-85-2 |2 NLM | |
650 | 7 | |a white sealant |2 NLM | |
650 | 7 | |a 91450-39-4 |2 NLM | |
700 | 1 | |a Gilpatrick, R O |e verfasserin |4 aut | |
700 | 1 | |a Moore, D |e verfasserin |4 aut | |
773 | 0 | 8 | |i Enthalten in |t The Journal of the Tennessee Dental Association |d 1993 |g 77(1997), 4 vom: 02. Okt., Seite 36-40 |w (DE-627)NLM00162069X |x 0040-3385 |7 nnns |
773 | 1 | 8 | |g volume:77 |g year:1997 |g number:4 |g day:02 |g month:10 |g pages:36-40 |
912 | |a GBV_USEFLAG_A | ||
912 | |a GBV_NLM | ||
951 | |a AR | ||
952 | |d 77 |j 1997 |e 4 |b 02 |c 10 |h 36-40 |